Preparation and Properties of Nano Lithium Magnesium Silicate-chitosan-sodium Alginate Composite Scaffold Materials

WANG Mingxia1,2, LIU Zhihui2, ZHU Zhen3, LI Lingfeng2, WANG Bowei1()   

  1. 1.The Second Hospital of Jilin University,Changchun 130021,China
    2.Hospital of Stomatology,Jilin University,Changchun 130021,China
    3.Zhenjiang Stomatological Hospital,Zhenjiang 212001,China
  • Received:2021-03-19 Online:2021-10-10 Published:2021-05-21
  • Contact: WANG Bowei E-mail:wangbw@jlu.edu.cn

Abstract:

Using vacuum freeze-drying technology, composite scaffolds were fabricated by mixing different mass fractions of nano-lithium magnesium silicate(nLMS) with chitosan and sodium alginate. Results showed that the composite scaffolds were porous solids possessing morphological plasticity, the longitudinal section of the composite scaffold was lamellar, the structure was loose and the internal pores were highly connected. With the increase of nLMS content, the porosity of the composite scaffold decreased and then increased. When the mass fraction of nLMS solution was 3%, both the swelling ratio and the degradation rate of the composite scaffold were the lowest. Besides, the addition of nLMS reduced the toxicity of the composite scaffold. The optimal mass fraction of nLMS solution to prepare the composite scaffold is 3%.

Key words: Bone tissue engineering, Scaffold, Chitosan, Sodium alginate, Lithium magnesium silicate