Solid-State 13C NMR Study of Pyrolytic Materials of Para-Cresol-formaldehyde Resin

XIE De-Min, ZHANG Jian-Guo, WANG Cun-Guo, WANG Rong-Shun   

  1. Department of Chemistry, Northeast Normal University, Changchun, 130024
  • Received:1993-07-07 Revised:1993-12-12 Online:1994-07-24 Published:1994-07-24

关键词: 对甲基酚醛树脂, 裂解, 固体13C, NMR

Abstract: 13C high-resolution solid-state NMRstudy has been performed with respect to polyacenic materials which were prepared by pyrolytic treatment of para-cresol-formaldehyde resin at different temperatures, The results show that with the increase of pyrolysis temperature, as the reaction of intermolecular dehydration and intramolecular dehydrogenation take place, a greater condensed aromatic ring is formed, so the chemical shifts exhibit an up-field shift.When the pyrolytic temperature reaches 900-1100℃, the main peak is composed of a group spectral lines continuously.This change can not be a chemical shift, it seems to be a Knight shift.

Key words: Para-cresol-formaldehyde resin, Pyrolysis, Solid-state 13C NMR