Chem. J. Chinese Universities ›› 2003, Vol. 24 ›› Issue (7): 1237.

• Preface • Previous Articles     Next Articles

Raman Spectroscopy of Titanium Dioxide Photocatalyst

WANG Jian-Qiang1, XIN Bai-Fu1, YU Hai-Tao1, XIE Yu-Tao2, ZHAO Bing2, FU Hong-Gang1   

  1. 1. Institute of Chemistry and Chemical Engineering, Heilongjiang University, Harbin 150080, China;
    2. Key Laboratory for Supramolecular Structure and Materials of Ministry of Education, Jilin University, Changchun 130023, China
  • Received:2002-02-27 Online:2003-07-24 Published:2003-07-24

Abstract: Nano-size TiO2, Fe3+-TiO2, TiO2/SiO2, and Fe3+-TiO2/SiO2 were prepared by sol-gel method. The structural change of TiO2 caused by different calcining conditions, Fe3+-doped contents, and formation of film on silica were studied by FT-Raman and confocal Raman technologies. The experimental results show that the different crystalline phases were observed at different calcinating temperatures. The titanium dioxide powder heated at 350-550 ℃ for two hours forms an anatase phase. The anatase phase materials transforms to rutile phase at 600 ℃ and transits completely to rutile phase calcining for two hours at 750 ℃. After doping Fe3+, the FWHM at 144cm-1 of Fe3+-TiO2 and Fe3+-TiO2/SiO2 is broadened apparently compared with that of TiO2 and TiO2/SiO2, respectively. Some peaks of TiO2/SiO2 coating film has some shift and broadening compared with those of TiO2.

Key words: Titanium dioxide, Raman spectrum, Doping, Coating film