摘要: 穆斯堡尔谱用于研究通水管道腐蚀产物,文献[1,2]有报导。腐蚀产物随着水中的杂质、水温及管道材料而异。
Abstract: The corrosion products, inside the branch pipes of geothermal power station in Fengshun of Guangdong, have been studied by absorption Mossbauer spectroscopy.The inlet branch is made of seamless steel tube and the outlet branch is made of cast iron. The corrosion product of the former is γ-FeOOH only, whereas the products of the latter are FeO(60%), Fe3O4 (31%) with small amount of γ-FeOOH(5%) and α-Fe2O3(4%).
TrendMD:
洪蕊玉, 郑裕芳, 范家师, 吴杰陶, 卢敬业, 张成周. 广东丰顺地热发电站通水管腐蚀产物的穆斯堡尔谱的研究. 高等学校化学学报, 1983, 4(5): 667.
Hong Ruiyu, Zheng Yufang, Fan Jiashi, Wu Jietao, Lu Jingye, Zhang Chengzhou. A MOSSBAUER SPECTROSCOPIC INVESTIGATION OF CORROSION PRODUCTS OF WATER-PIPES OF GEOTHERMAL POWER STATION. Chem. J. Chinese Universities, 1983, 4(5): 667.